Pin Hole Defect in Metallizing: 5 Ways to Eliminate Them Introduction:
Pin Hole Defect in Metallizing: 5 Ways to Eliminate Them
Introduction:
In vacuum metallizing, a layer of metal is deposited on a substrate. Better the deposition, better the film quality. Pin hole defect in metallizing, sometimes also referred as pin windows, are the areas where no metal has been deposited. These can be a big problem for quality metallizing especially in yarn grade metalizing where a pin hole can cause the thread to break. In others too, pin hole defect in metallizing can result in poor product quality, causing a huge loss of money. Pin hole defect in metallizing, sometimes also referred as pin windows, are the areas where no metal has been deposited. These can be a big problem for quality Metallizing especially